Mechanisms of Oxide Formation in the Self-Reacting Friction Stir Weld Process [STUB]

Abstract: The initial objective of this study was to evaluate the effect of an extended delay time between preweld cleaning and the completion of a self-reacting friction stir welding (SRFSW) process on the resulting quality of various thickness panels of AA2219-T87. The current NASA standard specifies no more than a 48 hour delay between preweld cleaning and actual welding. The concern is whether increasing the cleaning delay time results in development of the residual oxide defect (ROD) in SRFSW. Thi…